# (c) Silvaco Inc., 2025 # thinner ox/nitride on STI, thinner PR, thicker spacer, # ext anneal, thinner poly, multiple rotations on halo # Required Modules # Victory Process # -2D Diffusion & Implantation # Victory Mesh # -2D Meshing # Victory Device # -2D Simulator ####### PROCESS SIMULATION ####### GO victoryprocess simflags="-P 4" SET type = "NFET" SET t_gox = 0.03 SET vdd = 5.0 SET pitch = 15 SET Lgate = 5 SET Lcnt = ($pitch-$Lgate)/2 SET xmin = 0 SET xg = $Lgate/2 SET xmax = $xg + $Lcnt # thinner ox/nitride on STI, thinner PR, thicker spacer, # ext anneal, thinner poly, multiple rotations on halo INIT material="silicon" c.boron=1e16 from=$xmin to=$xmax depth=5 gasheight=2 resolution="0.1,0.02" meshdepth=3 flow.dim=2d # X-planes LINE x location = $xmin spacing = 0.1 LINE x location = $xg spacing = 0.02 LINE x location = $xmax spacing= 0.1 # Z-planes LINE z location = -0.5 spacing = 0.02 LINE z location = -0.03 spacing = 0.003 LINE z location = 0 spacing = 0.002 LINE z location = 0.1 spacing = 0.01 LINE z location = 1 spacing = 0.05 LINE z location = 5 spacing = 0.5 # DEPOSIT initial oxide layer DEPOSIT max material=oxide thickness=0.01 ## NWell IF cond = (@type = "PFET") IMPLANT Phosphorus energy=250 dose=1e13 tilt=0 IMPLANT Phosphorus energy=120 dose=1e13 tilt=0 IMPLANT Phosphorus energy=30 dose=2e13 tilt=0 IF.end DIFFUSE time=10 temp=1000 # sacrificial/scattering oxide ETCH oxide thick=0.011 dry DEPOSIT conformal material=oxide thicknes=0.01 # PMOS VT implant IF cond = (@type = "PFET") SET pvt_energy = 70 SET pvt_dose = 1.5e13 IMPLANT energy=$pvt_energy arsenic dose=$pvt_dose tilt=7.0 IF.end # Remove initial and sacrificial oxide layers ETCH wet material=oxide thick=0.012 # gate oxide DIFFUSE time=15 temp=850 weto2 SAVE name = PG-Fig2-25-Device_gox visualstr.conformal visualstr.nobackground go victoryprocess simflags="-P 4" LOAD name = PG-Fig2-25-Device_gox # Polygate definiton DEPOSIT conformal material=polysilicon thick=0.2 ETCH dry material="polysilicon" thick=0.25 right.to=$xg # open S/D windows (gate oxide), self-aligned to gate ETCH dry material=oxide thick=$t_gox*1.5 right.to=$xg #PMOS Halo implant IF cond = (@type = "PFET") SET phalo_energy = 34 SET phalo_dose = 7e13 SET phalo_tilt = 25 IMPLANT arsenic energy=$phalo_energy dose=$phalo_dose/2 tilt=$phalo_tilt rotation=0 BCA n.ion=10e3 traj.split plus.n IMPLANT arsenic energy=$phalo_energy dose=$phalo_dose/2 tilt=$phalo_tilt rotation=180 BCA n.ion=10e3 traj.split plus.n #PMOS extension implant SET pext_energy = 3 SET pext_dose = 2e14 IMPLANT energy=$pext_energy bf2 dose=$pext_dose tilt=7 rotation=0 IF.end SAVE name = PG-Fig2-25-Device_SD visualstr.conformal visualstr.nobackground go victoryprocess simflags="-P 4" LOAD name = PG-Fig2-25-Device_SD # NMOS-S/D phosphorus spin-on dopant (doped glass film) IF cond = (@type = "NFET") SET sod_t = 0.2 SET sod_p = 5e20 DEPOSIT conformal material=oxide thickness=$sod_t c.phosphorus=$sod_p IF.end # PMOS-S/D implantation IF cond = (@type = "PFET") SET pSD_dose = 1e15 SET pSD_energy = 3 IMPLANT energy=$pSD_energy bf2 dose=$pSD_dose tilt=7 rotation=0 IF.end SAVE name = PG-Fig2-25-Device_Back visualstr.conformal visualstr.nobackground go victoryprocess simflags="-P 4" LOAD name = PG-Fig2-25-Device_Back #SOD drive-in SET diff_temp = 1000 SET diff_time = 90 DIFFUSE temp=$diff_temp time=$diff_time # strip SOD glass ETCH dry material=oxide thick=$sod_t*1.1 # ILD: planarizing spin-on glass DEPOSIT material=oxide thick=0.0 max DEPOSIT material=oxide thickness=0.1 conformal ETCH dry material=oxide thick=0.4 angle=87 right.to=$xmax-2 DEPOSIT aluminum max thick=0 SAVE name=PG-Fig2-25-Device_cmos.str visualstr.conformal visualstr.nobackground SAVE name = PG-Fig2-25-Device_final visualstr.conformal visualstr.nobackground # Extraction of doping profile #### Device: Extraction #### go victoryextract simflags="-P 4" LOAD in = "PG-Fig2-25-Device_cmos_exVC.str" EXTRACT.profile name=Vgate regions=silicon field="net doping" x.val=$xmin csvfile=Vgate.csv EXTRACT.profile name=VsdN regions=silicon field="net doping" x.val=$xmax csvfile=Vsd.csv EXTRACT.profile name=Hsd regions=silicon field="net doping" y.val=0.05 csvfile=Hsd.csv ####### STRUCTURE REMESHING ####### go victorymesh simflags="-P 4" LOAD in = PG-Fig2-25-Device_final MATERIAL regions="polysilicon" value="Aluminum" CROP from="0.0" to="$xmax" MIRROR axes="-1x" REMESH delaunay REFINE max.size=0.2 regions="*" REFINE max.size=0.01 regions="oxide" REFINE max.junction.size=0.02 max.junction.distance.size=0.2 REFINE regions="silicon" interface.regions="sio2" max.interface.size=0.005 max.interface.distance.size=0.05 SAVE out = PG-Fig2-25-Device_mesh.str mode = VICTORY ####### DEVICE SIMULATION ####### go victorydevice simflags="-P 4" MESH infile = PG-Fig2-25-Device_mesh.str verbose = 3 #### STRUCTURE SPECIFICATION #### SET c1 = $xmax - 1 SET c2 = -1*$c1 ELECTRODE name=drain coor.region=($c2,-0.1,-0.1) ELECTRODE name=source coor.region=($c1,-0.1,-0.1) ELECTRODE name=gate coor.region=(0,-0.15,-0.15) ELECTRODE name=substrate bottom SET nWF = 4.1 SET pWF = 5.1 SET nvsat = 1e7 SET pvsat = 8e6 IF cond = (@type = "NFET") SET WF = $nWF SET sign = 1 ##!! SET vsat = $nvsat IF.end IF cond = (@type = "PFET") SET WF = $pWF SET sign = -1 ##!! SET vsat = $pvsat IF.end CONTACT name=gate workfunction=$WF CONTACT name=drain con.resist=1e-10 CONTACT name=source con.resist=1e-10 OUTPUT band.param con.band val.band recomb impact e.velocity h.velocity u.srh e.mobility e.temp h.mobility h.temp charge u.bbt #### MATERIAL/PHYSICAL MODELS #### MODELS cvt srh auger bgn print #### NUMERICAL METHODS #### METHOD newton trap maxtraps=8 c.tol=1.e-4 p.tol=1e-4 MATERIAL material=silicon taun0=1e-10 taup0=1e-10 MODELS fldmob MATERIAL vsat=$vsat # Fowler-Nordheim gate tunneling (for gate leakage) MODELS fnord #### SOLUTION SOLVING #### #IdVg_LIN LOG off SOLVE initial SOLVE previous SOLVE name = drain vdrain = 0 vstep = $sign*0.01 vfinal = $sign*0.05 LOG outf = PG-Fig2-25-Device_idvg_lin.log master SOLVE vgate = 0.0 vstep = $sign*0.02 vfinal = $sign*$vdd name = gate #IdVg_SAT LOG off SOLVE initial SOLVE previous SOLVE name = drain vdrain = 0 vstep = $sign*0.01 vfinal = $sign*$vdd LOG outf = PG-Fig2-25-Device_idvg_sat.log master SOLVE vgate = 0 vstep = $sign*0.02 vfinal = $sign*$vdd name = gate SAVE outfile = PG-Fig2-25-Device_idvg_sat.str #IdVd (Vg = Vdd) LOG off SOLVE initial SOLVE previous SOLVE name = gate vgate = 0 vstep = $sign*0.25 vfinal = $sign*$vdd LOG outf = PG-Fig2-25-Device_idvd.log master SOLVE name = drain vdrain = 0 vstep = $sign*0.1 vfinal = $sign*$vdd #IgVg (gate leakage, Vd = Vs = Vsub = 0) SET vgleak = 30 LOG off SOLVE initial SOLVE previous LOG outf = PG-Fig2-25-Device_igvg.log master SOLVE name = gate vgate = 0 vstep = $sign*0.5 vfinal = $sign*$vgleak victoryvisual PG-Fig2-25-Device_idvg_sat.str:PG-Fig2-25-Device_device.set victoryvisual PG-Fig2-25-Device_idvg_lin.log:PG-Fig2-25-Device_idvg.set+PG-Fig2-25-Device_idvg_sat.log:PG-Fig2-25-Device_idvg.set victoryvisual PG-Fig2-25-Device_idvd.log victoryvisual PG-Fig2-25-Device_igvg.log go victoryextract simflags="-P 4" SET Ivt = 1e-7/$Lgate SET width = 1 ##!! # Idvg_lin LOAD in = PG-Fig2-25-Device_idvg_lin.log SET X = "Gate Voltage" ##!! SET Y = "Drain Current" ##!! CURVE name = cv_idvg_lin x = "abs($X)" y = "abs($Y/$width)" # Vtlin at 100nA/um current EXTRACT.curve name = Vtlin_[V] expression = "intercept(y = $Ivt, curve.cv_idvg_lin)" # Vtgmax EXTRACT.maxslope.xintercept name = Vtx no.write EXTRACT.vdoe name = Vgmax_[V] expression = "$Vtx - 0.025" # Idlin per um EXTRACT.curve name = Idlin_[uA/um] expression = "1e6*intercept(x = $Vdd, curve.cv_idvg_lin)" #SSlin CURVE name = idvg_log x = "abs($X)" y = "log10(abs($Y/$width))" CURVE name = "log_slope" expression = "derivative(curve.idvg_log)" EXTRACT.curve name = slope expression = "intercept(x = 0.05, curve.log_slope)" no.write EXTRACT.vdoe name = SSlin_[mV/dec] expression = 1/$slope*1000 # idvg_sat # LOAD in = PG-Fig2-25-Device_idvg_sat.log SET X = "Gate Voltage" ##!! SET Y = "Drain Current" ##!! CURVE name = cv_idvg_sat x = "abs($X)" y = "abs($Y/$width)" EXTRACT.curve name = Vtsat_[V] expression = "intercept(y = $Ivt, curve.cv_idvg_sat)" # Idsat per um EXTRACT.curve name = Idsat_[uA/um] expression = "1e6*intercept(x = $Vdd, curve.cv_idvg_sat)" # Ioff per um EXTRACT.curve name = Ioff_[nA/um] expression = "1e9*intercept(x = 0.0, curve.cv_idvg_sat)" EXTRACT.vdoe name = LogIoff expression = "Log10($'Ioff_[nA/um]'*1e-9)" # SSsat CURVE name = idvg_log x = "abs($X)" y = "log10(abs($Y/$width))" CURVE name = "log_slope" expression = "derivative(curve.idvg_log)" EXTRACT.curve name = slope expression = "intercept(x = 0.05, curve.log_slope)" no.write EXTRACT.vdoe name = SSsat_[mV/dec] expression = 1/$slope*1000 EXTRACT.vdoe name = dibl_[mV] expression = 1e3*abs($'Vtsat_[V]' - $'Vtlin_[V]') # Gate leakage LOAD in = PG-Fig2-25-Device_igvg.log SET X = "Gate Voltage" ##!! SET Y = "Gate Current" ##!! CURVE name = cv_igvg x = "abs($X)" y = "abs($Y/$width)" EXTRACT.curve name = Ig_at_Vdd_[A/um] expression = "intercept(x = $Vdd, curve.cv_igvg)" QUIT