# ============================================================================= # CMOS INVERTER # ============================================================================= ####### PROCESS SIMULATION ####### GO victoryprocess simflags="-P 4" # ---------------- process knobs ---------------- SET sub_b = 1e15 # ASSUMED substrate boron /cm3 SET zmax = 8.0 # ASSUMED simulated depth (um); sheet: 525um SET wox_temp = 850 SET wox_time = 15 SET nit_t = 0.1 # LOCOS nitride mask thickness (um) SET rie_ox = 0.15 # ASSUMED oxide RIE depth (um) SET sod_t = 0.2 SET sod_p_well = 1e19 # ASSUMED - calibrate to measured Rs SET sod_p_sd = 5e20 # ASSUMED SET sod_b = 5e20 # ASSUMED SET boe_t = 0.25 SET dif_temp = 1000 SET dif_time = 90 SET poly_t = 0.2 SET cont_etch = 0.2 # ASSUMED SET al_t = 0.6 SET ovl = 0.5 # ASSUMED S/D window overlap onto gate edge (um) # ---------------- LAYOUT (um) ---------------- SET nw_a = 39 SET nw_b = 80 SET act_n_a = 3 SET act_n_b = 33 SET act_p_a = 44 SET act_p_b = 74 SET gn_a = 19 SET gn_b = 24 SET gp_a = 54 SET gp_b = 59 SET ptap_a = 3 SET ptap_b = 7 SET nsrc_a = 9 SET ndrn_b = 33 SET psrc_a = 44 SET pdrn_b = 68 SET ntap_a = 70 SET ntap_b = 74 SET nsrc_b = $gn_a+$ovl SET ndrn_a = $gn_b-$ovl SET psrc_b = $gp_a+$ovl SET pdrn_a = $gp_b-$ovl SET c_ptap_a = 4 SET c_ptap_b = 6 SET c_nsrc_a = 12 SET c_nsrc_b = 16 SET c_gn_a = 19.5 SET c_gn_b = 23.5 SET c_ndrn_a = 27 SET c_ndrn_b = 31 SET c_psrc_a = 47 SET c_psrc_b = 51 SET c_gp_a = 54.5 SET c_gp_b = 58.5 SET c_pdrn_a = 62 SET c_pdrn_b = 66 SET c_ntap_a = 71 SET c_ntap_b = 73 # ============================================================================= # 0. DOMAIN, MESH (step 0: p-type substrate) # ============================================================================= INIT material="silicon" c.boron=$sub_b from=0 to=84 depth=$zmax gasheight=2 \ resolution="0.5,0.05" meshdepth=2 flow.dim=2d LINE X location=0 spacing=1.0 LINE X location=3 spacing=0.5 LINE X location=9 spacing=0.5 LINE X location=19 spacing=0.4 LINE X location=24 spacing=0.4 LINE X location=33 spacing=0.5 LINE X location=39 spacing=1.0 LINE X location=44 spacing=0.5 LINE X location=54 spacing=0.4 LINE X location=59 spacing=0.4 LINE X location=68 spacing=0.5 LINE X location=74 spacing=0.5 LINE X location=80 spacing=1.0 LINE X location=84 spacing=1.0 LINE Z location=-0.5 spacing=0.05 LINE Z location=0 spacing=0.01 LINE Z location=0.5 spacing=0.05 LINE Z location=2.0 spacing=0.3 LINE Z location=$zmax spacing=2.0 # ============================================================================= # 1. n-WELL FORMATION (steps 1-12) # ============================================================================= DIFFUSE weto2 temperature=$wox_temp time=$wox_time # pad ox (sheet: 20nm) ETCH dry material=oxide between.x="$nw_a,$nw_b" thick=$rie_ox # open well window DEPOSIT material=oxide thickness=$sod_t phosphor=$sod_p_well conformal # VERIFY: SOD via Deposit DIFFUSE time=$dif_time temperature=$dif_temp # inert drive-in ETCH wet material=oxide thick=$boe_t # BOE strips SOD glass + pad ox STRIP material=oxide # clean-up -> bare silicon SAVE name=cmos_1_nwell visualstr.conformal visualstr.nobackground # ============================================================================= # 2. ACTIVE AREA (LOCOS) (steps 13-18) # ============================================================================= DEPOSIT conformal material=nitride thick=$nit_t ETCH dry material=nitride between.x="0,$act_n_a" thick=$nit_t ETCH dry material=nitride between.x="$act_n_b,$act_p_a" thick=$nit_t ETCH dry material=nitride between.x="$act_p_b,84" thick=$nit_t DIFFUSE weto2 temperature=$wox_temp time=$wox_time # field ox (sheet: 20nm) STRIP material=nitride SAVE name=cmos_2_locos visualstr.conformal visualstr.nobackground # ============================================================================= # 3. POLYSILICON GATE (steps 19-25) # ============================================================================= DIFFUSE weto2 temperature=$wox_temp time=$wox_time # gate ox (sheet target: 30nm) DEPOSIT conformal material=polysilicon thick=$poly_t ETCH dry material=polysilicon between.x="0,$gn_a" thick=$poly_t ETCH dry material=polysilicon between.x="$gn_b,$gp_a" thick=$poly_t ETCH dry material=polysilicon between.x="$gp_b,84" thick=$poly_t SAVE name=cmos_3_poly visualstr.conformal visualstr.nobackground # ============================================================================= # 4. n+ SOURCE/DRAIN (steps 26-35) NMOS S/D + n-well tap # ============================================================================= ETCH dry material=oxide between.x="$nsrc_a,$nsrc_b" thick=$rie_ox ETCH dry material=oxide between.x="$ndrn_a,$ndrn_b" thick=$rie_ox ETCH dry material=oxide between.x="$ntap_a,$ntap_b" thick=$rie_ox DEPOSIT material=oxide thickness=$sod_t phosphor=$sod_p_sd conformal DIFFUSE time=$dif_time temperature=$dif_temp ETCH wet material=oxide thick=$boe_t SAVE name=cmos_4_nplus visualstr.conformal visualstr.nobackground # ============================================================================= # 5. p+ SOURCE/DRAIN (steps 36-45) PMOS S/D + p-substrate tap # ============================================================================= ETCH dry material=oxide between.x="$ptap_a,$ptap_b" thick=$rie_ox ETCH dry material=oxide between.x="$psrc_a,$psrc_b" thick=$rie_ox ETCH dry material=oxide between.x="$pdrn_a,$pdrn_b" thick=$rie_ox DEPOSIT material=oxide thickness=$sod_t boron=$sod_b conformal DIFFUSE time=$dif_time temperature=$dif_temp ETCH wet material=oxide thick=$boe_t SAVE name=cmos_5_pplus visualstr.conformal visualstr.nobackground # ============================================================================= # 6. CONTACT HOLES (steps 46-51) # ============================================================================= DIFFUSE weto2 temperature=$wox_temp time=$wox_time # cover ox (sheet: 20nm) ETCH dry material=oxide between.x="$c_ptap_a,$c_ptap_b" thick=$cont_etch ETCH dry material=oxide between.x="$c_nsrc_a,$c_nsrc_b" thick=$cont_etch ETCH dry material=oxide between.x="$c_gn_a,$c_gn_b" thick=$cont_etch ETCH dry material=oxide between.x="$c_ndrn_a,$c_ndrn_b" thick=$cont_etch ETCH dry material=oxide between.x="$c_psrc_a,$c_psrc_b" thick=$cont_etch ETCH dry material=oxide between.x="$c_gp_a,$c_gp_b" thick=$cont_etch ETCH dry material=oxide between.x="$c_pdrn_a,$c_pdrn_b" thick=$cont_etch ETCH dry material=oxide between.x="$c_ntap_a,$c_ntap_b" thick=$cont_etch # ============================================================================= # 7. METALLIZATION (steps 52-53) Al 600nm, lift-off # ============================================================================= DEPOSIT conformal material=aluminum thick=$al_t ETCH dry material=aluminum between.x="0,$c_gn_a" thick=$al_t ETCH dry material=aluminum between.x="$c_gn_b,$c_gp_a" thick=$al_t ETCH dry material=aluminum between.x="$c_gp_b,$c_ndrn_a" thick=$al_t ETCH dry material=aluminum between.x="$c_ndrn_b,$c_nsrc_a" thick=$al_t ETCH dry material=aluminum between.x="$c_nsrc_b,$c_ntap_a" thick=$al_t ETCH dry material=aluminum between.x="$c_ntap_b,$c_pdrn_a" thick=$al_t ETCH dry material=aluminum between.x="$c_pdrn_b,$c_psrc_a" thick=$al_t ETCH dry material=aluminum between.x="$c_psrc_b,$c_ptap_a" thick=$al_t ETCH dry material=aluminum between.x="$c_ptap_b,84" thick=$al_t SAVE name=cmos_inverter_final visualstr.conformal visualstr.nobackground # ============================================================================= # STRUCTURE REMESHING # ============================================================================= GO victorymesh simflags="-P 4" LOAD in = cmos_inverter_final REMESH delaunay REFINE max.size=0.5 regions="*" REFINE max.junction.size=0.05 max.junction.distance.size=0.5 SAVE out = cmos_inverter_device.str mode = VICTORY # ============================================================================= # DEVICE TEST: inverter VTC # ============================================================================= GO victorydevice simflags="-P 4" MESH infile = cmos_inverter_device.str verbose=3 #### STRUCTURE SPECIFICATION #### ELECTRODE name=ss coor.region=(5,0,0) ELECTRODE name=ss coor.region=(14,0,0) ELECTRODE name=gate coor.region=(21.5,0,0) ELECTRODE name=gate coor.region=(56.5,0,0) ELECTRODE name=out coor.region=(29,0,0) ELECTRODE name=out coor.region=(64,0,0) ELECTRODE name=dd coor.region=(49,0,0) ELECTRODE name=dd coor.region=(72,0,0) CONTACT name=ss con.resist=1e-10 CONTACT name=dd con.resist=1e-10 CONTACT name=out con.resist=1e-10 SET gateWF = 4.6 CONTACT name=gate workfunction=$gateWF OUTPUT band.param con.band val.band recomb e.mobility h.mobility charge #### MATERIAL/PHYSICAL MODELS #### MODELS cvt srh auger bgn print METHOD newton trap maxtraps=8 c.tol=1.e-4 p.tol=1e-4 #### SOLUTION: ramp VDD, then sweep input, output floats #### SET vsupply = 5.0 LOG off SOLVE initial SOLVE previous SOLVE name=dd vdd=0.0 vstep=0.25 vfinal=$vsupply LOG outf=cmos_inv_vtc.log master SOLVE vgate=0.0 vstep=0.05 vfinal=$vsupply name=gate QUIT