add final data
This commit is contained in:
@@ -1,16 +1,4 @@
|
||||
# Hacker Fab PMOS -- Al gate / Al2O3 gate dielectric -- Silvaco Victory flow
|
||||
# Layout: Pmos.gds (cell "Pmos", um) -- put it in the DeckBuild working dir.
|
||||
#
|
||||
# WHY THE PROCESS ORDER CHANGED vs. the poly-gate deck
|
||||
# Aluminum melts at 660 C, so the gate cannot exist during the 1100 C boron
|
||||
# drive-in. The flow is therefore "diffusion first, gate last":
|
||||
# S/D boron SOD (patterned) -> drive-in -> strip -> ALD Al2O3 -> Al gate
|
||||
# -> 700B SOG -> contacts (SOG + Al2O3) -> Al contacts / pads
|
||||
# The gate is no longer self-aligned: it overlaps the S/D only because the
|
||||
# boron spreads laterally under the gate edge during the drive-in. GateOv
|
||||
# (S/D mask offset) and SDTime set that overlap.
|
||||
# Victory Process cannot anneal once Al2O3 is in the structure (material
|
||||
# table: Al2O3 diffusion "-"), which this order also respects.
|
||||
#
|
||||
# Masks (GDS layer -> Victory Process mask name "L#<layer>.<datatype>")
|
||||
# Pattern 1 S/D boron SOD diff 65/20 AND NOT poly 66/20 (2 etches)
|
||||
|
||||
Reference in New Issue
Block a user