# ===== VICTORY DoE GOLDEN DECK (3D) -- generated from hackerfab_pmos_al.in ===== # Do not edit by hand: edit the DeckBuild deck and regenerate with make_doe.py. # Put Pmos.gds in the project drop zone as a supplemental file. # Split variables (all others are #vpm_fix): Qf, RhoSub, Tsod, Csod_B, SDTime, SDTemp, GateOv, Tal2o3. # 3D: run process/mesh nodes ONE at a time (each is near the ~2.1 GB # session limit). Device modules are lighter and may run in parallel. # Hacker Fab PMOS -- Al gate / Al2O3 gate dielectric -- Silvaco Victory flow # Layout: Pmos.gds (cell "Pmos", um) -- put it in the DeckBuild working dir. # # WHY THE PROCESS ORDER CHANGED vs. the poly-gate deck # Aluminum melts at 660 C, so the gate cannot exist during the 1100 C boron # drive-in. The flow is therefore "diffusion first, gate last": # S/D boron SOD (patterned) -> drive-in -> strip -> ALD Al2O3 -> Al gate # -> 700B SOG -> contacts (SOG + Al2O3) -> Al contacts / pads # The gate is no longer self-aligned: it overlaps the S/D only because the # boron spreads laterally under the gate edge during the drive-in. GateOv # (S/D mask offset) and SDTime set that overlap. # Victory Process cannot anneal once Al2O3 is in the structure (material # table: Al2O3 diffusion "-"), which this order also respects. # # Masks (GDS layer -> Victory Process mask name "L#.") # Pattern 1 S/D boron SOD diff 65/20 AND NOT poly 66/20 (2 etches) # Pattern 2 Al gate poly 66/20 (Al kept inside polygons) # Pattern 3 Contacts li1 67/20 REVERSE (SOG + Al2O3 opened inside) # Pattern 4 Contact metal met1 68/20 (Al kept inside polygons) # Not used: nwell (wafer is n-type), psdm/nsdm, mcon (0.28 um, below litho). # # Gate dielectric: ALD Al2O3, material "Al2O3" (Victory Process material ID 229); # its permittivity is set to the ALD value (KAlOx) in the device modules. # If Victory Device rejects "Al2O3", replace every material=Al2O3 with # material=sapphire (the Al2O3 name both simulators are documented to know). # # Domain: transistor symmetric about x = 25 (gate centre) and y = 0. # 2D: x 25..38.5 cut at y = 0, mirrored in x. # 3D: x 25..38.5, y 0..7.5 after removing the uniform stripe y = 4..10 # (LAYOUT.REMOVE.Y), mirrored in x; y = 0 is a symmetry plane and # currents are normalized by the simulated half-width Wn = 6.5 um. # # Device simulation is split into three modules (transfer / output / gate # leakage). Each ends with a "go internal" DeckBuild extract block, so the same # extraction runs in DeckBuild and in Victory DoE (VDoE manual sec. 12.4). # In Victory DoE the three device modules can run in parallel. # # Conventions: cleans/resist/expose/develop/strip = comments; wet etches = # ETCH WET in 2D, ETCH DRY in 3D (memory); spin-on films = deposited oxide; # furnace steps = inert anneals. NEVER put a # comment on a line ending in "\". # -P N = threads. Session has ~4-5 cores and ~2.1 GB: 2D -P 4, 3D -P 1. GO victoryprocess simflags="-P 1" #global_var # Variables shared between modules (VDoE manual sec. 12.2) SET Lgate = 4.1667 # Drawn gate length #vpm_fix SET W = 25.0 # Gate width (diff y -12.5..12.5) #vpm_fix SET Ysq = 6.0 # width of the removed stripe (um) #vpm_fix SET Vdd = 5.0 #vpm_fix SET Vgleak = 10.0 # 10 V / 20 nm = 5 MV/cm (Al2O3 breaks down ~5-8 MV/cm) #vpm_fix SET WF = 4.1 # Al gate work function (eV) #vpm_fix SET KAlOx = 9.0 # ALD Al2O3 relative permittivity #vpm_fix SET Qf = -1.0e12 # Al2O3/Si fixed charge (cm^-2); ALD Al2O3 is negative SET Tau = 1.0e-6 # SRH lifetimes (s); realistic for a clean wafer #vpm_fix SET Wn = $W/2-$Ysq # 3D: simulated half-width (y = 0 symmetry plane, squeezed) #vpm_fix #global_var ## ---------------------------------- ## ## ------- Layout-derived geometry ---- ## ## -----------------------------------## SET Xg = 25.0 # Gate centre (poly 22.917..27.083) #vpm_fix SET Xge = $Xg+$Lgate/2 # Gate edge (27.083) #vpm_fix SET Xdiff = 37.5 # Diff edge in x #vpm_fix SET Ydiff = 12.5 # Diff edge in y #vpm_fix SET Xd = 33.333 # Drain contact centre (li1 31.667..35.0) #vpm_fix SET Xs = 16.667 # Source contact centre after mirroring #vpm_fix SET Xmax = 38.5 # Domain edge in x #vpm_fix SET Ymax = 13.5 # Domain edge in y (2D cut / unsqueezed) #vpm_fix # 3D "squeeze": the channel is uniform in y between the contacts/metal # (|y| <= 3.5) and the diff edge (12.5). LAYOUT.REMOVE.Y cuts y = 4..10 out of # the layout (manual: INIT LAYOUT.REMOVE.Y) and closes the gap, so the 3D # domain keeps every 3D feature (contacts, metal, diff edge, gate ends) with # ~45% less area. Simulated half-width = 12.5 - 6.0 = 6.5 um. ## ---------------------------------- ## ## ------- DOE process knobs ---------- ## ## -----------------------------------## SET RhoSub = 10 # n-type wafer resistivity (ohm-cm) SET Tsod = 0.25 # Boron SOD thickness (um) -- calibrate SET Csod_B = 5.0e20 # Boron SOD effective concentration -- calibrate to Rs SET SDTime = 30 # S/D drive-in time (min) SET SDTemp = 1100 # S/D drive-in temperature (C) SET GateOv = 0.0 # S/D mask pull-back from the drawn gate edge (um per # side). >0: S/D starts further from the gate (less # overlap); <0: S/D drawn under the gate. SET Tal2o3 = 0.020 # ALD Al2O3 gate dielectric thickness (um) ## ---------------------------------- ## ## ------- Other film parameters ------ ## ## -----------------------------------## SET TalG = 0.50 # Gate Al thickness (um), thermal evaporation #vpm_fix SET GateBias = 0.0 # Gate mask bias (um per edge, DELTACD) #vpm_fix SET Tsog = 0.30 # 700B SOG thickness (um) -- calibrate #vpm_fix SET Tal = 0.50 # Contact Al thickness (um) #vpm_fix SET AlBias = 0.0 # Contact-metal mask bias (met1 encloses li1 by 1.83 um) #vpm_fix ## ---------------------------------- ## ## ------- Wet-etch model ------------ ## ## -----------------------------------## # 2D: ETCH WET (isotropic). 3D: ETCH DRY (WET over 3D topography runs out of # memory). The gate Al wet etch undercuts by ~its thickness; in 3D that undercut # is reproduced by shrinking the gate mask (GateUC) so 2D and 3D gates match. SET etchm = "dry" #vpm_fix SET Tclr = 0.02 #vpm_fix SET TclrAl = 0.10+$TalG+$Tsog #vpm_fix SET GateUC = $TalG+0.05 #vpm_fix ## ---------------------------------- ## ## -------- Step 0: Substrate -------- ## ## -----------------------------------## # n-type wafer; native oxide removed by the BOE dip before the SOD spin. # Grid: finest cell = resolution/16 (meshdepth=3) must be <= ~1/1.5 of the # thinnest layer (20 nm Al2O3; manual sec. 2.10.3). # 2D 0.16 -> 10 nm. 3D "0.32, 0.40, 0.21" -> 20 / 25 / 13 nm (low accuracy, # fits ~2.1 GB). Gas height 3 um holds the stack (1.32 um) plus the barrier # layer masked ETCH WET deposits. INIT material=silicon orientation=100 dopants=phosphorus resistivity=$RhoSub \ depth=3.0 gasHeight=3.0 LAYOUT="Pmos.gds" CELL="Pmos" \ LAYOUT.REMOVE.Y="4.0, 10.0" \ FROM="25.0,0.0" TO="38.5,7.5" FLOW.DIM=3D \ resolution="0.32, 0.40, 0.21" meshdepth=3 # Doping (volume-data) mesh SET sxg = 0.20 #vpm_fix SET sxd = 0.30 #vpm_fix SET szs = 0.03 #vpm_fix SET szj = 0.08 #vpm_fix LINE x location=$Xg spacing=0.5 LINE x location=$Xge spacing=$sxg LINE x location=$Xge+1.5 spacing=0.4 LINE x location=$Xdiff spacing=$sxd LINE x location=$Xmax spacing=0.5 LINE y location=0 spacing=1.5 LINE y location=$Ydiff-$Ysq spacing=0.4 LINE y location=$Ymax-$Ysq spacing=0.5 LINE z location=-3.0 spacing=0.50 LINE z location=-1.5 spacing=0.20 LINE z location=-0.55 spacing=0.10 LINE z location=0.0 spacing=$szs LINE z location=0.3 spacing=$szj LINE z location=1.5 spacing=0.15 LINE z location=3.0 spacing=0.50 ## ---------------------------------- ## ## ---- S/D boron SOD (pattern 1) ---- ## ## -----------------------------------## # Acetone + IPA clean; BOE dip (native oxide) (no-op) # Spin-on dopant (boron, e.g. Filmtronics B153/B155), 4000 rpm, 20 s DEPOSIT conformal material=oxide thickness=$Tsod dopants=boron dopingvalues=$Csod_B # HMDS / spin AZ P4210 / bake / stepper litho -- Pattern 1: S/D = diff NOT gate # Develop, then BOE 6:1 10 s removes the SOD outside the S/D windows: # (a) outside diff ETCH $etchm material=oxide thickness=$Tsod+$Tclr MASK="L#65.20" # (b) over the gate area (poly polygon grown by GateOv per side) ETCH $etchm material=oxide thickness=$Tsod+$Tclr MASK="L#66.20" REVERSE DELTACD=$GateOv # Wet strip resist (no-op) # S/D drive-in, inert (tube furnace) # AUTOREF=false: keep the grid fixed during the anneal (inert, no moving # surfaces; adaptive refinement only costs memory). DIFFUSE time=$SDTime min temperature=$SDTemp AUTOREF=false # BOE 6:1, 10 min -- strip SOD glass ETCH $etchm material=oxide thickness=$Tsod+$Tclr SAVE name=HF_PMOS_Al_VP_SD ## ---------------------------------- ## ## ---- Gate stack (pattern 2) ------- ## ## -----------------------------------## # ALD Al2O3 gate dielectric (no anneals are possible after this point) DEPOSIT conformal material=Al2O3 thickness=$Tal2o3 # Thermal evaporation Al (gate) DEPOSIT conformal material=aluminum thickness=$TalG # HMDS / spin / bake / stepper litho -- Pattern 2: gate (poly 66/20) / develop # Type A Al etchant, 40 C -- keep Al inside the gate polygons; stops on Al2O3. ETCH $etchm material=aluminum thickness=$TalG+0.05 MASK="L#66.20" DELTACD=$GateBias-$GateUC # Wet strip resist (no-op) SAVE name=HF_PMOS_Al_VP_Gate ## ---------------------------------- ## ## ---- ILD + contacts (pattern 3) --- ## ## -----------------------------------## # Spin-coat 700B SOG, 4000 rpm, 20 s (modeled conformal). # The 200 C / 10 min bake is omitted: thermally negligible, and Victory Process # cannot run DIFFUSE with Al2O3 in the structure. DEPOSIT conformal material=oxide thickness=$Tsog # HMDS / spin / bake / stepper litho -- Pattern 3: contacts (li1 67/20) / develop # BOE 6:1 -- open SOG, then Al2O3, inside the contact polygons ETCH $etchm material=oxide thickness=$Tsog+$Tclr MASK="L#67.20" REVERSE ETCH $etchm material=Al2O3 thickness=$Tal2o3+0.005 MASK="L#67.20" REVERSE # Wet strip resist (no-op) SAVE name=HF_PMOS_Al_VP_Contact ## ---------------------------------- ## ## ---- Contact metal (pattern 4) ---- ## ## -----------------------------------## # Thermal evaporation Al DEPOSIT conformal material=aluminum thickness=$Tal # Clean / spin / bake / stepper litho -- Pattern 4: metal (met1 68/20) / develop # Type A Al etchant -- keep Al inside met1 (gate Al is protected by the SOG) ETCH $etchm material=aluminum thickness=$Tal+$TclrAl MASK="L#68.20" DELTACD=$AlBias # Wet strip resist (no-op) SAVE name=HF_PMOS_Al_VP_Metal ## ---------------------------------- ## ## ------ Mirror & electrodes -------- ## ## -----------------------------------## MIRROR mirror="-x" ELECTRODES name=gate x=$Xg+0.5 y=0.5 z=-($Tal2o3+$TalG/2) ELECTRODES name=source x=$Xs y=0.5 z=-0.1 ELECTRODES name=drain x=$Xd y=0.5 z=-0.1 ELECTRODES substrate SAVE name=HF_PMOS_Al_VP_sv GO victorymesh simflags="-P 1" ####### STRUCTURE REMESHING ####### LOAD in=HF_PMOS_Al_VP_sv # Junction is ~1-1.5 um deep; 2.5 um keeps it with margin and trims the mesh. CROP axis = "z" offset = "2.5" REMESH conformal SAVE out=HF_PMOS_Al_VM_con.str ####### DEVICE SIMULATION ####### # Three modules: (A) transfer, (B) output, (C) gate leakage. All biases are # negative (PMOS). Coarse bias steps on purpose (speed). ## ===== (A) Transfer: Id-Vg at Vd = -Vdlin and Vd = -Vdd ===== ## GO victorydevice simflag="-P 2" SET Vgmax = 2.0 # sweeps start at +2 V (off) and go to -Vdd #vpm_fix SET Vdlin = 0.1 #vpm_fix MESH infile=HF_PMOS_Al_VM_con.str CONTACT name=gate workfunction=$WF MATERIAL material=Al2O3 permittivity=$KAlOx INTERFACE qf=$Qf MATERIAL material=silicon taun0=$Tau taup0=$Tau MODELS fermi srh cvt fldmob print METHOD newton maxtrap=10 SOLVE init SOLVE previous SOLVE vstep=0.5 vfinal=$Vgmax name=gate SOLVE vdrain=-0.01 SOLVE vstep=-0.05 vfinal=-$Vdlin name=drain SAVE outfile=tA_lowD SOLVE vstep=-$Vdd/5 vfinal=-$Vdd name=drain SAVE outfile=tA_highD LOAD infile=tA_lowD LOG outfile=@cnode_HF_PMOS_Al_VD_IdVg_lin.log SOLVE vstep=-0.25 vfinal=-$Vdd name=gate LOG off LOAD infile=tA_highD LOG outfile=@cnode_HF_PMOS_Al_VD_IdVg_sat.log SOLVE vstep=-0.25 vfinal=-$Vdd name=gate LOG off go internal # Signed PMOS values (Vt negative). Currents normalized to A/um via Wn. SET Io = 1e-7 #vpm_fix extract init infile="@pnode_HF_PMOS_Al_VD_IdVg_lin.log" extract name="Vtgm_V" (xintercept(minslope(curve(v."gate",abs(i."drain")))) - ave(v."drain")/2.0) extract name="Vtlin_V" x.val from curve(v."gate",abs(i."drain")) where y.val=$Io*$Wn/$Lgate extract name="Idlin_A" y.val from curve(v."gate",abs(i."drain")) where x.val=-$Vdd extract name="Idlin_uA_um" $"Idlin_A"*1e6/$Wn extract init infile="@pnode_HF_PMOS_Al_VD_IdVg_sat.log" extract name="Vtsat_V" x.val from curve(v."gate",abs(i."drain")) where y.val=$Io*$Wn/$Lgate extract name="Idsat_A" y.val from curve(v."gate",abs(i."drain")) where x.val=-$Vdd extract name="Idsat_uA_um" $"Idsat_A"*1e6/$Wn extract name="Ioff_A" y.val from curve(v."gate",abs(i."drain")) where x.val=0.0 extract name="Ioff_pA_um" $"Ioff_A"*1e12/$Wn extract name="SSsat_mV_dec" -1000.0/slope(minslope(curve(v."gate",log10(abs(i."drain"))))) extract name="DIBL_mV" ($"Vtsat_V" - $"Vtlin_V")*1000.0 ## ===== (B) Output: Id-Vd, Vg = -1 .. -5 V ===== ## GO victorydevice simflag="-P 2" MESH infile=HF_PMOS_Al_VM_con.str CONTACT name=gate workfunction=$WF MATERIAL material=Al2O3 permittivity=$KAlOx INTERFACE qf=$Qf MATERIAL material=silicon taun0=$Tau taup0=$Tau MODELS fermi srh cvt fldmob print METHOD newton maxtrap=10 SOLVE init SOLVE previous SAVE outfile=tB_zero LOAD infile=tB_zero SOLVE vstep=-0.5 vfinal=-1.0 name=gate LOG outfile=@cnode_HF_PMOS_Al_VD_IdVd_Vg1.log SOLVE vdrain=0.0 SOLVE vstep=-0.5 vfinal=-$Vdd name=drain LOG off LOAD infile=tB_zero SOLVE vstep=-0.5 vfinal=-2.0 name=gate LOG outfile=@cnode_HF_PMOS_Al_VD_IdVd_Vg2.log SOLVE vdrain=0.0 SOLVE vstep=-0.5 vfinal=-$Vdd name=drain LOG off LOAD infile=tB_zero SOLVE vstep=-0.5 vfinal=-3.0 name=gate LOG outfile=@cnode_HF_PMOS_Al_VD_IdVd_Vg3.log SOLVE vdrain=0.0 SOLVE vstep=-0.5 vfinal=-$Vdd name=drain LOG off LOAD infile=tB_zero SOLVE vstep=-0.5 vfinal=-4.0 name=gate LOG outfile=@cnode_HF_PMOS_Al_VD_IdVd_Vg4.log SOLVE vdrain=0.0 SOLVE vstep=-0.5 vfinal=-$Vdd name=drain LOG off LOAD infile=tB_zero SOLVE vstep=-0.5 vfinal=-5.0 name=gate LOG outfile=@cnode_HF_PMOS_Al_VD_IdVd_Vg5.log SOLVE vdrain=0.0 SOLVE vstep=-0.5 vfinal=-$Vdd name=drain LOG off go internal extract init infile="@pnode_HF_PMOS_Al_VD_IdVd_Vg5.log" extract name="IdVd5_A" max(abs(i."drain")) extract name="IdVd5_uA_um" $"IdVd5_A"*1e6/$Wn ## ===== (C) Gate leakage: Ig-Vg, Vd = Vs = Vsub = 0 ===== ## # Fowler-Nordheim tunneling only in this module (it slows every solve). # Note: the built-in FN coefficients are for SiO2; for Al2O3 (lower barrier) # the absolute Ig is indicative only -- compare trends between splits. GO victorydevice simflag="-P 2" MESH infile=HF_PMOS_Al_VM_con.str CONTACT name=gate workfunction=$WF MATERIAL material=Al2O3 permittivity=$KAlOx INTERFACE qf=$Qf MATERIAL material=silicon taun0=$Tau taup0=$Tau MODELS fermi srh cvt fldmob fn.cur print METHOD newton maxtrap=10 SOLVE init SOLVE previous LOG outfile=@cnode_HF_PMOS_Al_VD_IgVg.log SOLVE vstep=-1.0 vfinal=-$Vgleak name=gate LOG off go internal extract init infile="@pnode_HF_PMOS_Al_VD_IgVg.log" extract name="Ig_Vdd_A" y.val from curve(v."gate",abs(i."gate")) where x.val=-$Vdd extract name="Ig_Vgleak_A" y.val from curve(v."gate",abs(i."gate")) where x.val=-$Vgleak quit