223 lines
9.3 KiB
Plaintext
223 lines
9.3 KiB
Plaintext
# =============================================================================
|
|
# CMOS INVERTER
|
|
# =============================================================================
|
|
|
|
####### PROCESS SIMULATION #######
|
|
GO victoryprocess simflags="-P 4"
|
|
|
|
# ---------------- process knobs ----------------
|
|
SET sub_b = 1e15 # ASSUMED substrate boron /cm3
|
|
SET zmax = 8.0 # ASSUMED simulated depth (um); sheet: 525um
|
|
SET wox_temp = 850
|
|
SET wox_time = 15
|
|
SET nit_t = 0.1 # LOCOS nitride mask thickness (um)
|
|
SET rie_ox = 0.15 # ASSUMED oxide RIE depth (um)
|
|
SET sod_t = 0.2
|
|
SET sod_p_well = 1e19 # ASSUMED - calibrate to measured Rs
|
|
SET sod_p_sd = 5e20 # ASSUMED
|
|
SET sod_b = 5e20 # ASSUMED
|
|
SET boe_t = 0.25
|
|
SET dif_temp = 1000
|
|
SET dif_time = 90
|
|
SET poly_t = 0.2
|
|
SET cont_etch = 0.2 # ASSUMED
|
|
SET al_t = 0.6
|
|
SET ovl = 0.5 # ASSUMED S/D window overlap onto gate edge (um)
|
|
|
|
# ---------------- LAYOUT (um) ----------------
|
|
SET nw_a = 39
|
|
SET nw_b = 80
|
|
SET act_n_a = 3
|
|
SET act_n_b = 33
|
|
SET act_p_a = 44
|
|
SET act_p_b = 74
|
|
SET gn_a = 19
|
|
SET gn_b = 24
|
|
SET gp_a = 54
|
|
SET gp_b = 59
|
|
SET ptap_a = 3
|
|
SET ptap_b = 7
|
|
SET nsrc_a = 9
|
|
SET ndrn_b = 33
|
|
SET psrc_a = 44
|
|
SET pdrn_b = 68
|
|
SET ntap_a = 70
|
|
SET ntap_b = 74
|
|
SET nsrc_b = $gn_a+$ovl
|
|
SET ndrn_a = $gn_b-$ovl
|
|
SET psrc_b = $gp_a+$ovl
|
|
SET pdrn_a = $gp_b-$ovl
|
|
SET c_ptap_a = 4
|
|
SET c_ptap_b = 6
|
|
SET c_nsrc_a = 12
|
|
SET c_nsrc_b = 16
|
|
SET c_gn_a = 19.5
|
|
SET c_gn_b = 23.5
|
|
SET c_ndrn_a = 27
|
|
SET c_ndrn_b = 31
|
|
SET c_psrc_a = 47
|
|
SET c_psrc_b = 51
|
|
SET c_gp_a = 54.5
|
|
SET c_gp_b = 58.5
|
|
SET c_pdrn_a = 62
|
|
SET c_pdrn_b = 66
|
|
SET c_ntap_a = 71
|
|
SET c_ntap_b = 73
|
|
|
|
# =============================================================================
|
|
# 0. DOMAIN, MESH (step 0: p-type substrate)
|
|
# =============================================================================
|
|
INIT material="silicon" c.boron=$sub_b from=0 to=84 depth=$zmax gasheight=2 \
|
|
resolution="0.5,0.05" meshdepth=2 flow.dim=2d
|
|
|
|
LINE X location=0 spacing=1.0
|
|
LINE X location=3 spacing=0.5
|
|
LINE X location=9 spacing=0.5
|
|
LINE X location=19 spacing=0.4
|
|
LINE X location=24 spacing=0.4
|
|
LINE X location=33 spacing=0.5
|
|
LINE X location=39 spacing=1.0
|
|
LINE X location=44 spacing=0.5
|
|
LINE X location=54 spacing=0.4
|
|
LINE X location=59 spacing=0.4
|
|
LINE X location=68 spacing=0.5
|
|
LINE X location=74 spacing=0.5
|
|
LINE X location=80 spacing=1.0
|
|
LINE X location=84 spacing=1.0
|
|
LINE Z location=-0.5 spacing=0.05
|
|
LINE Z location=0 spacing=0.01
|
|
LINE Z location=0.5 spacing=0.05
|
|
LINE Z location=2.0 spacing=0.3
|
|
LINE Z location=$zmax spacing=2.0
|
|
|
|
# =============================================================================
|
|
# 1. n-WELL FORMATION (steps 1-12)
|
|
# =============================================================================
|
|
DIFFUSE weto2 temperature=$wox_temp time=$wox_time # pad ox (sheet: 20nm)
|
|
ETCH dry material=oxide between.x="$nw_a,$nw_b" thick=$rie_ox # open well window
|
|
DEPOSIT material=oxide thickness=$sod_t phosphor=$sod_p_well conformal # VERIFY: SOD via Deposit
|
|
DIFFUSE time=$dif_time temperature=$dif_temp # inert drive-in
|
|
ETCH wet material=oxide thick=$boe_t # BOE strips SOD glass + pad ox
|
|
STRIP material=oxide # clean-up -> bare silicon
|
|
SAVE name=cmos_1_nwell visualstr.conformal visualstr.nobackground
|
|
|
|
# =============================================================================
|
|
# 2. ACTIVE AREA (LOCOS) (steps 13-18)
|
|
# =============================================================================
|
|
DEPOSIT conformal material=nitride thick=$nit_t
|
|
ETCH dry material=nitride between.x="0,$act_n_a" thick=$nit_t
|
|
ETCH dry material=nitride between.x="$act_n_b,$act_p_a" thick=$nit_t
|
|
ETCH dry material=nitride between.x="$act_p_b,84" thick=$nit_t
|
|
DIFFUSE weto2 temperature=$wox_temp time=$wox_time # field ox (sheet: 20nm)
|
|
STRIP material=nitride
|
|
SAVE name=cmos_2_locos visualstr.conformal visualstr.nobackground
|
|
|
|
# =============================================================================
|
|
# 3. POLYSILICON GATE (steps 19-25)
|
|
# =============================================================================
|
|
DIFFUSE weto2 temperature=$wox_temp time=$wox_time # gate ox (sheet target: 30nm)
|
|
DEPOSIT conformal material=polysilicon thick=$poly_t
|
|
ETCH dry material=polysilicon between.x="0,$gn_a" thick=$poly_t
|
|
ETCH dry material=polysilicon between.x="$gn_b,$gp_a" thick=$poly_t
|
|
ETCH dry material=polysilicon between.x="$gp_b,84" thick=$poly_t
|
|
SAVE name=cmos_3_poly visualstr.conformal visualstr.nobackground
|
|
|
|
# =============================================================================
|
|
# 4. n+ SOURCE/DRAIN (steps 26-35) NMOS S/D + n-well tap
|
|
# =============================================================================
|
|
ETCH dry material=oxide between.x="$nsrc_a,$nsrc_b" thick=$rie_ox
|
|
ETCH dry material=oxide between.x="$ndrn_a,$ndrn_b" thick=$rie_ox
|
|
ETCH dry material=oxide between.x="$ntap_a,$ntap_b" thick=$rie_ox
|
|
DEPOSIT material=oxide thickness=$sod_t phosphor=$sod_p_sd conformal
|
|
DIFFUSE time=$dif_time temperature=$dif_temp
|
|
ETCH wet material=oxide thick=$boe_t
|
|
SAVE name=cmos_4_nplus visualstr.conformal visualstr.nobackground
|
|
|
|
# =============================================================================
|
|
# 5. p+ SOURCE/DRAIN (steps 36-45) PMOS S/D + p-substrate tap
|
|
# =============================================================================
|
|
ETCH dry material=oxide between.x="$ptap_a,$ptap_b" thick=$rie_ox
|
|
ETCH dry material=oxide between.x="$psrc_a,$psrc_b" thick=$rie_ox
|
|
ETCH dry material=oxide between.x="$pdrn_a,$pdrn_b" thick=$rie_ox
|
|
DEPOSIT material=oxide thickness=$sod_t boron=$sod_b conformal
|
|
DIFFUSE time=$dif_time temperature=$dif_temp
|
|
ETCH wet material=oxide thick=$boe_t
|
|
SAVE name=cmos_5_pplus visualstr.conformal visualstr.nobackground
|
|
|
|
# =============================================================================
|
|
# 6. CONTACT HOLES (steps 46-51)
|
|
# =============================================================================
|
|
DIFFUSE weto2 temperature=$wox_temp time=$wox_time # cover ox (sheet: 20nm)
|
|
ETCH dry material=oxide between.x="$c_ptap_a,$c_ptap_b" thick=$cont_etch
|
|
ETCH dry material=oxide between.x="$c_nsrc_a,$c_nsrc_b" thick=$cont_etch
|
|
ETCH dry material=oxide between.x="$c_gn_a,$c_gn_b" thick=$cont_etch
|
|
ETCH dry material=oxide between.x="$c_ndrn_a,$c_ndrn_b" thick=$cont_etch
|
|
ETCH dry material=oxide between.x="$c_psrc_a,$c_psrc_b" thick=$cont_etch
|
|
ETCH dry material=oxide between.x="$c_gp_a,$c_gp_b" thick=$cont_etch
|
|
ETCH dry material=oxide between.x="$c_pdrn_a,$c_pdrn_b" thick=$cont_etch
|
|
ETCH dry material=oxide between.x="$c_ntap_a,$c_ntap_b" thick=$cont_etch
|
|
|
|
# =============================================================================
|
|
# 7. METALLIZATION (steps 52-53) Al 600nm, lift-off
|
|
# =============================================================================
|
|
DEPOSIT conformal material=aluminum thick=$al_t
|
|
ETCH dry material=aluminum between.x="0,$c_gn_a" thick=$al_t
|
|
ETCH dry material=aluminum between.x="$c_gn_b,$c_gp_a" thick=$al_t
|
|
ETCH dry material=aluminum between.x="$c_gp_b,$c_ndrn_a" thick=$al_t
|
|
ETCH dry material=aluminum between.x="$c_ndrn_b,$c_nsrc_a" thick=$al_t
|
|
ETCH dry material=aluminum between.x="$c_nsrc_b,$c_ntap_a" thick=$al_t
|
|
ETCH dry material=aluminum between.x="$c_ntap_b,$c_pdrn_a" thick=$al_t
|
|
ETCH dry material=aluminum between.x="$c_pdrn_b,$c_psrc_a" thick=$al_t
|
|
ETCH dry material=aluminum between.x="$c_psrc_b,$c_ptap_a" thick=$al_t
|
|
ETCH dry material=aluminum between.x="$c_ptap_b,84" thick=$al_t
|
|
SAVE name=cmos_inverter_final visualstr.conformal visualstr.nobackground
|
|
|
|
# =============================================================================
|
|
# STRUCTURE REMESHING
|
|
# =============================================================================
|
|
GO victorymesh simflags="-P 4"
|
|
LOAD in = cmos_inverter_final
|
|
REMESH delaunay
|
|
REFINE max.size=0.5 regions="*"
|
|
REFINE max.junction.size=0.05 max.junction.distance.size=0.5
|
|
SAVE out = cmos_inverter_device.str mode = VICTORY
|
|
|
|
# =============================================================================
|
|
# DEVICE TEST: inverter VTC
|
|
# =============================================================================
|
|
GO victorydevice simflags="-P 4"
|
|
MESH infile = cmos_inverter_device.str verbose=3
|
|
|
|
#### STRUCTURE SPECIFICATION ####
|
|
ELECTRODE name=ss coor.region=(5,0,0)
|
|
ELECTRODE name=ss coor.region=(14,0,0)
|
|
ELECTRODE name=gate coor.region=(21.5,0,0)
|
|
ELECTRODE name=gate coor.region=(56.5,0,0)
|
|
ELECTRODE name=out coor.region=(29,0,0)
|
|
ELECTRODE name=out coor.region=(64,0,0)
|
|
ELECTRODE name=dd coor.region=(49,0,0)
|
|
ELECTRODE name=dd coor.region=(72,0,0)
|
|
|
|
CONTACT name=ss con.resist=1e-10
|
|
CONTACT name=dd con.resist=1e-10
|
|
CONTACT name=out con.resist=1e-10
|
|
SET gateWF = 4.6
|
|
CONTACT name=gate workfunction=$gateWF
|
|
|
|
OUTPUT band.param con.band val.band recomb e.mobility h.mobility charge
|
|
|
|
#### MATERIAL/PHYSICAL MODELS ####
|
|
MODELS cvt srh auger bgn print
|
|
METHOD newton trap maxtraps=8 c.tol=1.e-4 p.tol=1e-4
|
|
|
|
#### SOLUTION: ramp VDD, then sweep input, output floats ####
|
|
SET vsupply = 5.0
|
|
LOG off
|
|
SOLVE initial
|
|
SOLVE previous
|
|
SOLVE name=dd vdd=0.0 vstep=0.25 vfinal=$vsupply
|
|
LOG outf=cmos_inv_vtc.log master
|
|
SOLVE vgate=0.0 vstep=0.05 vfinal=$vsupply name=gate
|
|
|
|
QUIT
|