# (c) Silvaco Inc., 2025
|
|
# thinner ox/nitride on STI, thinner PR, thicker spacer,
|
|
# ext anneal, thinner poly, multiple rotations on halo
|
|
|
|
# Required Modules
|
|
# Victory Process
|
|
# -2D Diffusion & Implantation
|
|
# Victory Mesh
|
|
# -2D Meshing
|
|
# Victory Device
|
|
# -2D Simulator
|
|
|
|
|
|
####### PROCESS SIMULATION #######
|
|
GO victoryprocess simflags="-P 4"
|
|
SET type = "NFET"
|
|
SET t_gox = 0.03
|
|
SET vdd = 5.0
|
|
SET pitch = 15
|
|
SET Lgate = 5
|
|
SET Lcnt = ($pitch-$Lgate)/2
|
|
SET xmin = 0
|
|
SET xg = $Lgate/2
|
|
SET xmax = $xg + $Lcnt
|
|
|
|
|
|
# thinner ox/nitride on STI, thinner PR, thicker spacer, # ext anneal, thinner poly, multiple rotations on halo
|
|
INIT material="silicon" c.boron=1e16 from=$xmin to=$xmax depth=5 gasheight=2 resolution="0.1,0.02" meshdepth=3 flow.dim=2d
|
|
|
|
# X-planes
|
|
LINE x location = $xmin spacing = 0.1
|
|
LINE x location = $xg spacing = 0.02
|
|
LINE x location = $xmax spacing= 0.1
|
|
|
|
# Z-planes
|
|
LINE z location = -0.5 spacing = 0.02
|
|
LINE z location = -0.03 spacing = 0.003
|
|
LINE z location = 0 spacing = 0.002
|
|
LINE z location = 0.1 spacing = 0.01
|
|
LINE z location = 1 spacing = 0.05
|
|
LINE z location = 5 spacing = 0.5
|
|
|
|
# DEPOSIT initial oxide layer
|
|
DEPOSIT max material=oxide thickness=0.01
|
|
|
|
## NWell
|
|
IF cond = (@type = "PFET")
|
|
IMPLANT Phosphorus energy=250 dose=1e13 tilt=0
|
|
IMPLANT Phosphorus energy=120 dose=1e13 tilt=0
|
|
IMPLANT Phosphorus energy=30 dose=2e13 tilt=0
|
|
IF.end
|
|
|
|
DIFFUSE time=10 temp=1000
|
|
|
|
# sacrificial/scattering oxide
|
|
ETCH oxide thick=0.011 dry
|
|
DEPOSIT conformal material=oxide thicknes=0.01
|
|
|
|
# PMOS VT implant
|
|
IF cond = (@type = "PFET")
|
|
SET pvt_energy = 70
|
|
SET pvt_dose = 1.5e13
|
|
IMPLANT energy=$pvt_energy arsenic dose=$pvt_dose tilt=7.0
|
|
IF.end
|
|
|
|
# Remove initial and sacrificial oxide layers
|
|
ETCH wet material=oxide thick=0.012
|
|
# gate oxide
|
|
DEPOSIT material=oxide conformal thickness=$t_gox
|
|
|
|
SAVE name = PG-Fig2-25-Device_gox visualstr.conformal visualstr.nobackground
|
|
|
|
|
|
go victoryprocess simflags="-P 4"
|
|
LOAD name = PG-Fig2-25-Device_gox
|
|
|
|
# Polygate definiton
|
|
DEPOSIT conformal material=polysilicon thick=0.2
|
|
ETCH dry material="polysilicon" thick=0.25 right.to=$xg
|
|
# open S/D windows (gate oxide), self-aligned to gate
|
|
ETCH dry material=oxide thick=$t_gox*1.5 right.to=$xg
|
|
|
|
#PMOS Halo implant
|
|
IF cond = (@type = "PFET")
|
|
SET phalo_energy = 34
|
|
SET phalo_dose = 7e13
|
|
SET phalo_tilt = 25
|
|
IMPLANT arsenic energy=$phalo_energy dose=$phalo_dose/2 tilt=$phalo_tilt rotation=0 BCA n.ion=10e3 traj.split plus.n
|
|
IMPLANT arsenic energy=$phalo_energy dose=$phalo_dose/2 tilt=$phalo_tilt rotation=180 BCA n.ion=10e3 traj.split plus.n
|
|
|
|
#PMOS extension implant
|
|
SET pext_energy = 3
|
|
SET pext_dose = 2e14
|
|
IMPLANT energy=$pext_energy bf2 dose=$pext_dose tilt=7 rotation=0
|
|
IF.end
|
|
|
|
|
|
SAVE name = PG-Fig2-25-Device_SD visualstr.conformal visualstr.nobackground
|
|
|
|
go victoryprocess simflags="-P 4"
|
|
LOAD name = PG-Fig2-25-Device_SD
|
|
|
|
# NMOS-S/D phosphorus spin-on dopant (doped glass film)
|
|
IF cond = (@type = "NFET")
|
|
SET sod_t = 0.2
|
|
SET sod_p = 5e20
|
|
DEPOSIT conformal material=oxide thickness=$sod_t c.phosphorus=$sod_p
|
|
IF.end
|
|
|
|
# PMOS-S/D implantation
|
|
IF cond = (@type = "PFET")
|
|
SET pSD_dose = 1e15
|
|
SET pSD_energy = 3
|
|
IMPLANT energy=$pSD_energy bf2 dose=$pSD_dose tilt=7 rotation=0
|
|
IF.end
|
|
|
|
SAVE name = PG-Fig2-25-Device_Back visualstr.conformal visualstr.nobackground
|
|
|
|
|
|
go victoryprocess simflags="-P 4"
|
|
LOAD name = PG-Fig2-25-Device_Back
|
|
|
|
#SOD drive-in
|
|
SET diff_temp = 1000
|
|
SET diff_time = 90
|
|
DIFFUSE temp=$diff_temp time=$diff_time
|
|
|
|
# strip SOD glass
|
|
ETCH dry material=oxide thick=$sod_t*1.1
|
|
|
|
# ILD: planarizing spin-on glass
|
|
DEPOSIT material=oxide thick=0.0 max
|
|
DEPOSIT material=oxide thickness=0.1 conformal
|
|
|
|
ETCH dry material=oxide thick=0.4 angle=87 right.to=$xmax-2
|
|
DEPOSIT aluminum max thick=0
|
|
|
|
SAVE name=PG-Fig2-25-Device_cmos.str visualstr.conformal visualstr.nobackground
|
|
SAVE name = PG-Fig2-25-Device_final visualstr.conformal visualstr.nobackground
|
|
# Extraction of doping profile
|
|
#### Device: Extraction ####
|
|
go victoryextract simflags="-P 4"
|
|
LOAD in = "PG-Fig2-25-Device_cmos_exVC.str"
|
|
EXTRACT.profile name=Vgate regions=silicon field="net doping" x.val=$xmin csvfile=Vgate.csv
|
|
EXTRACT.profile name=VsdN regions=silicon field="net doping" x.val=$xmax csvfile=Vsd.csv
|
|
EXTRACT.profile name=Hsd regions=silicon field="net doping" y.val=0.05 csvfile=Hsd.csv
|
|
|
|
####### STRUCTURE REMESHING #######
|
|
go victorymesh simflags="-P 4"
|
|
LOAD in = PG-Fig2-25-Device_final
|
|
MATERIAL regions="polysilicon" value="Aluminum"
|
|
|
|
CROP from="0.0" to="$xmax"
|
|
MIRROR axes="-1x"
|
|
|
|
REMESH delaunay
|
|
REFINE max.size=0.2 regions="*"
|
|
REFINE max.size=0.01 regions="oxide"
|
|
REFINE max.junction.size=0.02 max.junction.distance.size=0.2
|
|
REFINE regions="silicon" interface.regions="sio2" max.interface.size=0.005 max.interface.distance.size=0.05
|
|
|
|
SAVE out = PG-Fig2-25-Device_mesh.str mode = VICTORY
|
|
|
|
|
|
####### DEVICE SIMULATION #######
|
|
go victorydevice simflags="-P 4"
|
|
MESH infile = PG-Fig2-25-Device_mesh.str verbose = 3
|
|
|
|
#### STRUCTURE SPECIFICATION ####
|
|
SET c1 = $xmax - 1
|
|
SET c2 = -1*$c1
|
|
ELECTRODE name=drain coor.region=($c2,-0.1,-0.1)
|
|
ELECTRODE name=source coor.region=($c1,-0.1,-0.1)
|
|
ELECTRODE name=gate coor.region=(0,-0.15,-0.15)
|
|
ELECTRODE name=substrate bottom
|
|
|
|
SET nWF = 4.1
|
|
SET pWF = 5.1
|
|
SET nvsat = 1e7
|
|
SET pvsat = 8e6
|
|
|
|
IF cond = (@type = "NFET")
|
|
SET WF = $nWF
|
|
SET sign = 1 ##!!
|
|
SET vsat = $nvsat
|
|
IF.end
|
|
|
|
IF cond = (@type = "PFET")
|
|
SET WF = $pWF
|
|
SET sign = -1 ##!!
|
|
SET vsat = $pvsat
|
|
IF.end
|
|
|
|
CONTACT name=gate workfunction=$WF
|
|
CONTACT name=drain con.resist=1e-10
|
|
CONTACT name=source con.resist=1e-10
|
|
|
|
OUTPUT band.param con.band val.band recomb impact e.velocity h.velocity u.srh e.mobility e.temp h.mobility h.temp charge u.bbt
|
|
|
|
#### MATERIAL/PHYSICAL MODELS ####
|
|
MODELS cvt srh auger bgn print
|
|
#### NUMERICAL METHODS ####
|
|
METHOD newton trap maxtraps=8 c.tol=1.e-4 p.tol=1e-4
|
|
MATERIAL material=silicon taun0=1e-10 taup0=1e-10
|
|
MODELS fldmob
|
|
MATERIAL vsat=$vsat
|
|
# Fowler-Nordheim gate tunneling (for gate leakage)
|
|
MODELS fnord
|
|
|
|
|
|
#### SOLUTION SOLVING ####
|
|
#IdVg_LIN
|
|
LOG off
|
|
SOLVE initial
|
|
SOLVE previous
|
|
SOLVE name = drain vdrain = 0 vstep = $sign*0.01 vfinal = $sign*0.05
|
|
LOG outf = PG-Fig2-25-Device_idvg_lin.log master
|
|
SOLVE vgate = 0.0 vstep = $sign*0.05 vfinal = $sign*$vdd name = gate
|
|
|
|
#IdVg_SAT
|
|
LOG off
|
|
SOLVE initial
|
|
SOLVE previous
|
|
SOLVE name = drain vdrain = 0 vstep = $sign*0.1 vfinal = $sign*$vdd
|
|
LOG outf = PG-Fig2-25-Device_idvg_sat.log master
|
|
SOLVE vgate = 0 vstep = $sign*0.05 vfinal = $sign*$vdd name = gate
|
|
SAVE outfile = PG-Fig2-25-Device_idvg_sat.str
|
|
|
|
#IdVd_Vg1
|
|
LOG off
|
|
SOLVE initial
|
|
SOLVE previous
|
|
SOLVE name = gate vgate = 0 vstep = $sign*0.25 vfinal = $sign*1
|
|
LOG outf = PG-Fig2-25-Device_idvd_vg1.log master
|
|
SOLVE name = drain vdrain = 0 vstep = $sign*0.1 vfinal = $sign*$vdd
|
|
|
|
#IdVd_Vg2
|
|
LOG off
|
|
SOLVE initial
|
|
SOLVE previous
|
|
SOLVE name = gate vgate = 0 vstep = $sign*0.25 vfinal = $sign*2
|
|
LOG outf = PG-Fig2-25-Device_idvd_vg2.log master
|
|
SOLVE name = drain vdrain = 0 vstep = $sign*0.1 vfinal = $sign*$vdd
|
|
|
|
#IdVd_Vg3
|
|
LOG off
|
|
SOLVE initial
|
|
SOLVE previous
|
|
SOLVE name = gate vgate = 0 vstep = $sign*0.25 vfinal = $sign*3
|
|
LOG outf = PG-Fig2-25-Device_idvd_vg3.log master
|
|
SOLVE name = drain vdrain = 0 vstep = $sign*0.1 vfinal = $sign*$vdd
|
|
|
|
#IdVd_Vg4
|
|
LOG off
|
|
SOLVE initial
|
|
SOLVE previous
|
|
SOLVE name = gate vgate = 0 vstep = $sign*0.25 vfinal = $sign*4
|
|
LOG outf = PG-Fig2-25-Device_idvd_vg4.log master
|
|
SOLVE name = drain vdrain = 0 vstep = $sign*0.1 vfinal = $sign*$vdd
|
|
|
|
#IdVd_Vg5
|
|
LOG off
|
|
SOLVE initial
|
|
SOLVE previous
|
|
SOLVE name = gate vgate = 0 vstep = $sign*0.25 vfinal = $sign*5
|
|
LOG outf = PG-Fig2-25-Device_idvd_vg5.log master
|
|
SOLVE name = drain vdrain = 0 vstep = $sign*0.1 vfinal = $sign*$vdd
|
|
|
|
#IgVg (gate leakage, Vd = Vs = Vsub = 0)
|
|
SET vgleak = 30
|
|
LOG off
|
|
SOLVE initial
|
|
SOLVE previous
|
|
LOG outf = PG-Fig2-25-Device_igvg.log master
|
|
SOLVE name = gate vgate = 0 vstep = $sign*0.5 vfinal = $sign*$vgleak
|
|
victoryvisual PG-Fig2-25-Device_idvg_sat.str:PG-Fig2-25-Device_device.set
|
|
victoryvisual PG-Fig2-25-Device_idvg_lin.log:PG-Fig2-25-Device_idvg.set+PG-Fig2-25-Device_idvg_sat.log:PG-Fig2-25-Device_idvg.set
|
|
victoryvisual PG-Fig2-25-Device_idvd_vg1.log+PG-Fig2-25-Device_idvd_vg2.log+PG-Fig2-25-Device_idvd_vg3.log+PG-Fig2-25-Device_idvd_vg4.log+PG-Fig2-25-Device_idvd_vg5.log
|
|
victoryvisual PG-Fig2-25-Device_igvg.log
|
|
|
|
|
|
go victoryextract simflags="-P 4"
|
|
SET Ivt = 1e-7/$Lgate
|
|
SET width = 1 ##!!
|
|
# Idvg_lin
|
|
LOAD in = PG-Fig2-25-Device_idvg_lin.log
|
|
|
|
SET X = "Gate Voltage" ##!!
|
|
SET Y = "Drain Current" ##!!
|
|
CURVE name = cv_idvg_lin x = "abs($X)" y = "abs($Y/$width)"
|
|
|
|
# Vtlin at 100nA/um current
|
|
EXTRACT.curve name = Vtlin_[V] expression = "intercept(y = $Ivt, curve.cv_idvg_lin)"
|
|
|
|
# Vtgmax
|
|
EXTRACT.maxslope.xintercept name = Vtx no.write
|
|
EXTRACT.vdoe name = Vgmax_[V] expression = "$Vtx - 0.025"
|
|
|
|
# Idlin per um
|
|
EXTRACT.curve name = Idlin_[uA/um] expression = "1e6*intercept(x = $Vdd, curve.cv_idvg_lin)"
|
|
|
|
# gm at Vg = Vdd
|
|
CURVE name = gm_lin expression = "derivative(curve.cv_idvg_lin)"
|
|
EXTRACT.curve name = gm_[uS/um] expression = "1e6*intercept(x = $Vdd, curve.gm_lin)"
|
|
|
|
#SSlin
|
|
CURVE name = idvg_log x = "abs($X)" y = "log10(abs($Y/$width))"
|
|
CURVE name = "log_slope" expression = "derivative(curve.idvg_log)"
|
|
EXTRACT.curve name = slope expression = "intercept(x = 0.05, curve.log_slope)" no.write
|
|
EXTRACT.vdoe name = SSlin_[mV/dec] expression = 1/$slope*1000
|
|
|
|
|
|
# idvg_sat
|
|
#
|
|
LOAD in = PG-Fig2-25-Device_idvg_sat.log
|
|
SET X = "Gate Voltage" ##!!
|
|
SET Y = "Drain Current" ##!!
|
|
CURVE name = cv_idvg_sat x = "abs($X)" y = "abs($Y/$width)"
|
|
EXTRACT.curve name = Vtsat_[V] expression = "intercept(y = $Ivt, curve.cv_idvg_sat)"
|
|
# Idsat per um
|
|
EXTRACT.curve name = Idsat_[uA/um] expression = "1e6*intercept(x = $Vdd, curve.cv_idvg_sat)"
|
|
# Ioff per um
|
|
EXTRACT.curve name = Ioff_[nA/um] expression = "1e9*intercept(x = 0.0, curve.cv_idvg_sat)"
|
|
EXTRACT.vdoe name = LogIoff expression = "Log10($'Ioff_[nA/um]'*1e-9)"
|
|
|
|
# SSsat
|
|
CURVE name = idvg_log x = "abs($X)" y = "log10(abs($Y/$width))"
|
|
CURVE name = "log_slope" expression = "derivative(curve.idvg_log)"
|
|
EXTRACT.curve name = slope expression = "intercept(x = 0.05, curve.log_slope)" no.write
|
|
EXTRACT.vdoe name = SSsat_[mV/dec] expression = 1/$slope*1000
|
|
|
|
EXTRACT.vdoe name = dibl_[mV] expression = 1e3*abs($'Vtsat_[V]' - $'Vtlin_[V]')
|
|
EXTRACT.vdoe name = LogIonIoff expression = "Log10(($'Idsat_[uA/um]'*1e-6)/($'Ioff_[nA/um]'*1e-9))"
|
|
|
|
# IdVd: Ron (Vg = 5 V, near origin)
|
|
LOAD in = PG-Fig2-25-Device_idvd_vg5.log
|
|
SET X = "Drain Voltage" ##!!
|
|
SET Y = "Drain Current" ##!!
|
|
CURVE name = cv_idvd_vg5 x = "abs($X)" y = "abs($Y/$width)"
|
|
CURVE name = gd_vg5 expression = "derivative(curve.cv_idvd_vg5)"
|
|
EXTRACT.curve name = gd_[uS/um] expression = "1e6*intercept(x = 0.1, curve.gd_vg5)"
|
|
EXTRACT.vdoe name = Ron_[kOhm.um] expression = "1e3/$'gd_[uS/um]'"
|
|
|
|
# IdVd: lambda (Vg = 2 V, Vd = 4 V in saturation)
|
|
LOAD in = PG-Fig2-25-Device_idvd_vg2.log
|
|
SET X = "Drain Voltage" ##!!
|
|
SET Y = "Drain Current" ##!!
|
|
CURVE name = cv_idvd_vg2 x = "abs($X)" y = "abs($Y/$width)"
|
|
CURVE name = gds_vg2 expression = "derivative(curve.cv_idvd_vg2)"
|
|
EXTRACT.curve name = Id_vd4_[uA/um] expression = "1e6*intercept(x = 4.0, curve.cv_idvd_vg2)"
|
|
EXTRACT.curve name = gds_[uS/um] expression = "1e6*intercept(x = 4.0, curve.gds_vg2)"
|
|
EXTRACT.vdoe name = lambda_[1/V] expression = "$'gds_[uS/um]'/$'Id_vd4_[uA/um]'"
|
|
|
|
# Gate leakage
|
|
LOAD in = PG-Fig2-25-Device_igvg.log
|
|
SET X = "Gate Voltage" ##!!
|
|
SET Y = "Gate Current" ##!!
|
|
CURVE name = cv_igvg x = "abs($X)" y = "abs($Y/$width)"
|
|
EXTRACT.curve name = Ig_at_Vdd_[A/um] expression = "intercept(x = $Vdd, curve.cv_igvg)"
|
|
EXTRACT.curve name = Ig_at_Vgleak_[A/um] expression = "intercept(x = $vgleak, curve.cv_igvg)"
|
|
|
|
QUIT
|