# CMOS INVERTER
# =============================================================================
####### PROCESS SIMULATION #######
GO victoryprocess simflags="-P 4"
# ---------------- process knobs ----------------
SET sub_b = 1e15 # ASSUMED substrate boron /cm3
SET zmax = 8.0 # ASSUMED simulated depth (um); sheet: 525um
SET wox_temp = 850
SET wox_time = 15
SET nit_t = 0.1 # LOCOS nitride mask thickness (um)
SET rie_ox = 0.15 # ASSUMED oxide RIE depth (um)
SET sod_t = 0.2
SET sod_p_well = 1e19 # ASSUMED - calibrate to measured Rs
SET sod_p_sd = 5e20 # ASSUMED
SET sod_b = 5e20 # ASSUMED
SET boe_t = 0.25
SET dif_temp = 1000
SET dif_time = 90
SET poly_t = 0.2
SET cont_etch = 0.2 # ASSUMED
SET al_t = 0.6
SET ovl = 0.5 # ASSUMED S/D window overlap onto gate edge (um)
# ---------------- LAYOUT (um) ----------------
SET nw_a = 39
SET nw_b = 80
SET act_n_a = 3
SET act_n_b = 33
SET act_p_a = 44
SET act_p_b = 74
SET gn_a = 19
SET gn_b = 24
SET gp_a = 54
SET gp_b = 59
SET ptap_a = 3
SET ptap_b = 7
SET nsrc_a = 9
SET ndrn_b = 33
SET psrc_a = 44
SET pdrn_b = 68
SET ntap_a = 70
SET ntap_b = 74
SET nsrc_b = $gn_a+$ovl
SET ndrn_a = $gn_b-$ovl
SET psrc_b = $gp_a+$ovl
SET pdrn_a = $gp_b-$ovl
SET c_ptap_a = 4
SET c_ptap_b = 6
SET c_nsrc_a = 12
SET c_nsrc_b = 16
SET c_gn_a = 19.5
SET c_gn_b = 23.5
SET c_ndrn_a = 27
SET c_ndrn_b = 31
SET c_psrc_a = 47
SET c_psrc_b = 51
SET c_gp_a = 54.5
SET c_gp_b = 58.5
SET c_pdrn_a = 62
SET c_pdrn_b = 66
SET c_ntap_a = 71
SET c_ntap_b = 73
# =============================================================================
# 0. DOMAIN, MESH (step 0: p-type substrate)
# =============================================================================
INIT material="silicon" c.boron=$sub_b from=0 to=84 depth=$zmax gasheight=2 \
resolution="0.5,0.05" meshdepth=2 flow.dim=2d
LINE X location=0 spacing=1.0
LINE X location=3 spacing=0.5
LINE X location=9 spacing=0.5
LINE X location=19 spacing=0.4
LINE X location=24 spacing=0.4
LINE X location=33 spacing=0.5
LINE X location=39 spacing=1.0
LINE X location=44 spacing=0.5
LINE X location=54 spacing=0.4
LINE X location=59 spacing=0.4
LINE X location=68 spacing=0.5
LINE X location=74 spacing=0.5
LINE X location=80 spacing=1.0
LINE X location=84 spacing=1.0
LINE Z location=-0.5 spacing=0.05
LINE Z location=0 spacing=0.01
LINE Z location=0.5 spacing=0.05
LINE Z location=2.0 spacing=0.3
LINE Z location=$zmax spacing=2.0
# =============================================================================
# 1. n-WELL FORMATION (steps 1-12)
# =============================================================================
DIFFUSE weto2 temperature=$wox_temp time=$wox_time # pad ox (sheet: 20nm)
ETCH dry material=oxide between.x="$nw_a,$nw_b" thick=$rie_ox # open well window
DEPOSIT material=oxide thickness=$sod_t phosphor=$sod_p_well conformal # VERIFY: SOD via Deposit
DIFFUSE time=$dif_time temperature=$dif_temp # inert drive-in
ETCH wet material=oxide thick=$boe_t # BOE strips SOD glass + pad ox
STRIP material=oxide # clean-up -> bare silicon
SAVE name=cmos_1_nwell visualstr.conformal visualstr.nobackground
# =============================================================================
# 2. ACTIVE AREA (LOCOS) (steps 13-18)
# =============================================================================
DEPOSIT conformal material=nitride thick=$nit_t
ETCH dry material=nitride between.x="0,$act_n_a" thick=$nit_t
ETCH dry material=nitride between.x="$act_n_b,$act_p_a" thick=$nit_t
ETCH dry material=nitride between.x="$act_p_b,84" thick=$nit_t
DIFFUSE weto2 temperature=$wox_temp time=$wox_time # field ox (sheet: 20nm)
STRIP material=nitride
SAVE name=cmos_2_locos visualstr.conformal visualstr.nobackground
# =============================================================================
# 3. POLYSILICON GATE (steps 19-25)
# =============================================================================
DIFFUSE weto2 temperature=$wox_temp time=$wox_time # gate ox (sheet target: 30nm)
DEPOSIT conformal material=polysilicon thick=$poly_t
ETCH dry material=polysilicon between.x="0,$gn_a" thick=$poly_t
ETCH dry material=polysilicon between.x="$gn_b,$gp_a" thick=$poly_t
ETCH dry material=polysilicon between.x="$gp_b,84" thick=$poly_t
SAVE name=cmos_3_poly visualstr.conformal visualstr.nobackground
# =============================================================================
# 4. n+ SOURCE/DRAIN (steps 26-35) NMOS S/D + n-well tap
# =============================================================================
ETCH dry material=oxide between.x="$nsrc_a,$nsrc_b" thick=$rie_ox
ETCH dry material=oxide between.x="$ndrn_a,$ndrn_b" thick=$rie_ox
ETCH dry material=oxide between.x="$ntap_a,$ntap_b" thick=$rie_ox
DEPOSIT material=oxide thickness=$sod_t phosphor=$sod_p_sd conformal
DIFFUSE time=$dif_time temperature=$dif_temp
ETCH wet material=oxide thick=$boe_t
SAVE name=cmos_4_nplus visualstr.conformal visualstr.nobackground
# =============================================================================
# 5. p+ SOURCE/DRAIN (steps 36-45) PMOS S/D + p-substrate tap
# =============================================================================
ETCH dry material=oxide between.x="$ptap_a,$ptap_b" thick=$rie_ox
ETCH dry material=oxide between.x="$psrc_a,$psrc_b" thick=$rie_ox
ETCH dry material=oxide between.x="$pdrn_a,$pdrn_b" thick=$rie_ox
DEPOSIT material=oxide thickness=$sod_t boron=$sod_b conformal
DIFFUSE time=$dif_time temperature=$dif_temp
ETCH wet material=oxide thick=$boe_t
SAVE name=cmos_5_pplus visualstr.conformal visualstr.nobackground
# =============================================================================
# 6. CONTACT HOLES (steps 46-51)
# =============================================================================
DIFFUSE weto2 temperature=$wox_temp time=$wox_time # cover ox (sheet: 20nm)
ETCH dry material=oxide between.x="$c_ptap_a,$c_ptap_b" thick=$cont_etch
ETCH dry material=oxide between.x="$c_nsrc_a,$c_nsrc_b" thick=$cont_etch
ETCH dry material=oxide between.x="$c_gn_a,$c_gn_b" thick=$cont_etch
ETCH dry material=oxide between.x="$c_ndrn_a,$c_ndrn_b" thick=$cont_etch
ETCH dry material=oxide between.x="$c_psrc_a,$c_psrc_b" thick=$cont_etch
ETCH dry material=oxide between.x="$c_gp_a,$c_gp_b" thick=$cont_etch
ETCH dry material=oxide between.x="$c_pdrn_a,$c_pdrn_b" thick=$cont_etch
ETCH dry material=oxide between.x="$c_ntap_a,$c_ntap_b" thick=$cont_etch
# =============================================================================
# 7. METALLIZATION (steps 52-53) Al 600nm, lift-off
# =============================================================================
DEPOSIT conformal material=aluminum thick=$al_t
ETCH dry material=aluminum between.x="0,$c_gn_a" thick=$al_t
ETCH dry material=aluminum between.x="$c_gn_b,$c_gp_a" thick=$al_t
ETCH dry material=aluminum between.x="$c_gp_b,$c_ndrn_a" thick=$al_t
ETCH dry material=aluminum between.x="$c_ndrn_b,$c_nsrc_a" thick=$al_t
ETCH dry material=aluminum between.x="$c_nsrc_b,$c_ntap_a" thick=$al_t
ETCH dry material=aluminum between.x="$c_ntap_b,$c_pdrn_a" thick=$al_t
ETCH dry material=aluminum between.x="$c_pdrn_b,$c_psrc_a" thick=$al_t
ETCH dry material=aluminum between.x="$c_psrc_b,$c_ptap_a" thick=$al_t
ETCH dry material=aluminum between.x="$c_ptap_b,84" thick=$al_t
SAVE name=cmos_inverter_final visualstr.conformal visualstr.nobackground
# =============================================================================
# STRUCTURE REMESHING
# =============================================================================
GO victorymesh simflags="-P 4"
LOAD in = cmos_inverter_final
REMESH delaunay
REFINE max.size=0.5 regions="*"
REFINE max.junction.size=0.05 max.junction.distance.size=0.5
SAVE out = cmos_inverter_device.str mode = VICTORY
# =============================================================================
# DEVICE TEST: inverter VTC
# =============================================================================
GO victorydevice simflags="-P 4"
MESH infile = cmos_inverter_device.str verbose=3
#### STRUCTURE SPECIFICATION ####
ELECTRODE name=ss coor.region=(5,0,0)
ELECTRODE name=ss coor.region=(14,0,0)
ELECTRODE name=gate coor.region=(21.5,0,0)
ELECTRODE name=gate coor.region=(56.5,0,0)
ELECTRODE name=out coor.region=(29,0,0)
ELECTRODE name=out coor.region=(64,0,0)
ELECTRODE name=dd coor.region=(49,0,0)
ELECTRODE name=dd coor.region=(72,0,0)
CONTACT name=ss con.resist=1e-10
CONTACT name=dd con.resist=1e-10
CONTACT name=out con.resist=1e-10
SET gateWF = 4.6
CONTACT name=gate workfunction=$gateWF
OUTPUT band.param con.band val.band recomb e.mobility h.mobility charge
#### MATERIAL/PHYSICAL MODELS ####
MODELS cvt srh auger bgn print
METHOD newton trap maxtraps=8 c.tol=1.e-4 p.tol=1e-4
#### SOLUTION: ramp VDD, then sweep input, output floats ####
SET vsupply = 5.0
LOG off
SOLVE initial
SOLVE previous
SOLVE name=dd vdd=0.0 vstep=0.25 vfinal=$vsupply
LOG outf=cmos_inv_vtc.log master
SOLVE vgate=0.0 vstep=0.05 vfinal=$vsupply name=gate
QUIT